Base oil
Technical description
Grades - SN 150, SN500
TEST |
UNITS |
METHODS |
SN 150 |
SN 500 |
---|---|---|---|---|
Density |
@ 15 °C |
ASTM-D 4052 |
- |
- |
Colour |
- Max |
ASTM-D 1500 |
1 |
2 |
Flash Point COC |
- Min°C |
ASTM-D 92 |
210 |
227 |
Flash Point PMCC |
- Min°C |
ASTM-D 93 |
200+ |
210+ |
Furfural Content |
- Max |
PPMM- 1414 |
5 |
5 |
Pour Point |
- Max°C |
ASTM-D 97 |
-12 |
-6 |
Viscosity @ 40 °C |
Cst |
ASTM-D 445 |
28/31 |
91/101 |
Viscosity @ 100 °C |
Cst |
ASTM-D 445 |
- |
- |
Viscosity Index |
- Min |
ASTM-D 2270 |
95 |
95 |
Carbon Residue |
- MaxWT % |
ASTM-D 189 |
- |
0.1 |
Sulphur Content |
- Max WT% |
ASTM-D 4294 |
0.6 |
1 |
Neutralization No |
- MaxMG KOH/GM |
ASTM-D 664 |
0.05 |
0.05 |
Copper Strip Corrosion |
- Max100 °C/3 Hrs |
ASTM-D 130 |
1A |
1A |
Ash- Max |
WT % |
ASTM-D 482 |
0.01 |
0.01 |
Appearance |
- |
Visual |
C&B |
C&B |