Bitumen
PRODUCT AT KHARG PETROCHEMICAL COMPANY
Technical description
Bitumen (40 / 50)
Description |
Unit |
Specification |
Test Method |
---|---|---|---|
Specific Gravity@ 25oC |
)Kg/m³( |
1.00 - 1.06 |
ASTM - D – 70 |
Penetration @ 25oC , 100gr. 5S |
0.1 mm) |
40 – 50 |
ASTM - D – 5 |
Softening Point |
)oC( |
52 – 60v |
ASTM - D – 36 |
Ductility@ 25oC |
)cm( |
Min. 100 |
ASTM - D – 113 |
Loss on Heating |
)% Wt( |
Max. 0.5 |
ASTM - D – 6 |
Drop in Penetration after Heating |
)%( |
Max. 20 |
ASTM - D –113, D-6, D-5 |
Flash Point |
)oC( |
Min. 250 |
ASTM - D – 92 |
Bitumen Content in CS2 |
)% Wt( |
Min. 99.00 |
ASTM - D – 4 |
Spot Test |
Negative |
A.A.S.H.O.T.102* |
Bitumen (60 / 70)
Description |
UNITS |
Specification |
Test Method |
|
---|---|---|---|---|
Specific Gravity@ 25 o C |
)Kg/m³( |
1.00 - 1.06 |
ASTM - D – 70 |
|
Penetration @ 25 o C |
(0.1 mm) |
60-70 |
ASTM - D – 5 |
|
Softening Point |
) o C( |
49 – 56 |
ASTM - D – 36 |
|
Ductility@ 25 o C |
)cm( |
Min. 100 |
ASTM - D – 113 |
|
Loss on Heating |
)% Wt( |
Max. 0.5 |
ASTM - D – 6 |
|
Drop in Penetration after Heating |
)%( |
Max. 20 |
ASTM - D –113, D-6, D-5 |
|
Flash Point |
) o C( |
Min. 250 |
ASTM - D – 92 |
|
Bitumen Content in CS2 |
)% Wt( |
Min. 99.00 |
ASTM - D – 4 |
|
Spot Test |
Negative |
A.A.S.H.O.T.102* |
Bitumen (80 / 100)
Description |
UNITS |
Specification |
Test Method |
|
---|---|---|---|---|
Specific Gravity @ 25 o C |
)Kg/m³( |
1.00 - 1.06 |
ASTM - D – 70 |
|
Penetration @ 25 o C |
(0.1 mm) |
80-100 |
ASTM - D – 5 |
|
Softening Point |
) o C( |
Min. 43 |
ASTM - D – 36 |
|
Ductility@ 25 o C |
)cm( |
Min. 100 |
ASTM - D – 113 |
|
Loss on Heating |
)% Wt( |
Max. 0.5 |
ASTM - D – 6 |
|
Drop in Penetration after Heating |
)%( |
Max. 20 |
ASTM - D –113, D-6, D-5 |
|
Flash Point |
) o C( |
Min. 225 |
ASTM - D – 92 |
|
Bitumen Content in CS2 |
)% Wt( |
Min. 99.00 |
ASTM - D – 4 |
|
Spot Test |
Negative |
A.A.S.H.O.T.102* |
Bitumen (85 / 100)
Description |
UNITS |
Specification |
Test Method |
|
---|---|---|---|---|
Specific Gravity @ 25 o C |
)Kg/m³( |
1.00 - 1.06 |
ASTM - D – 70 |
|
Penetration @ 25 o C |
(0.1 mm) |
85-100 |
ASTM - D – 5 |
|
Softening Point |
) o C( |
45-52 |
ASTM - D – 36 |
|
Ductility@ 25 o C |
)cm( |
Min. 100 |
ASTM - D – 113 |
|
Loss on Heating |
)% Wt( |
Max. 0.5 |
ASTM - D – 6 |
|
Drop in Penetration after Heating |
)%( |
Max. 20 |
ASTM - D –113, D-6, D-5 |
|
Flash Point |
) o C( |
Min. 225 |
ASTM - D – 92 |
|
Bitumen Content in CS2 |
)% Wt( |
Min. 99.5 |
ASTM - D – 4 |
|
Spot Test |
Negative |
A.A.S.H.O.T.102* |